Pond Waterproof HDPE Geomembrane Pit Liner

Pruduction Feature:1. Complete range of amplitude and thickness.2. Excellent environmental stress crack resistance and excellent chemical resistance.3. Excellent chemical resistance.4. Has a large operating temperature range and a long service life.5. Used in landfills, tailings storage sites, channel seepage prevention, dam see

Featured Products

Pruduction Feature:

1. Complete range of amplitude and thickness.
2. Excellent environmental stress crack resistance and excellent chemical resistance.
3. Excellent chemical resistance.
4. Has a large operating temperature range and a long service life.
5. Used in landfills, tailings storage sites, channel seepage prevention, dam seepage prevention and subway engineering, etc.

Geomembrane Applications

Flexible membranes are used in a variety of applications, such as:
A. Landfill lining and capping
B. Reservoirs, lagoons, ponds and lakes
C. Storm water attenuation
D. Hydrocarbon barrier
E. Impermeable liner
F. Dielectric membrane
Geomembrane Impermeable Black Industrial Pond Liner Geomembrane Price
Waterproofing HDPE Geo Membrane Pit Liner for Pond
Waterproofing HDPE Geo Membrane Pit Liner for Pond
Waterproofing HDPE Geo Membrane Pit Liner for Pond
Waterproofing HDPE Geo Membrane Pit Liner for Pond
Performance Index:
PropertiesTest Value
0.75mm1.00 mm1.50 mm2.00 mm
Thickness - mils (min. ave.)· lowest individual of 10 valuesnom. (mil)-10%nom. (mil)-10%nom. (mil)-10%nom. (mil)-10%
Density (min.)0.940 g/cc0.940 g/cc0.940 g/cc0.940 g/cc
Tensile Properties (1) (min. ave.)·  
 yield strength· 
 break strength· 
 yield elongation· 
 break elongation
11 kN/m
20 kN/m
12%
700%
15 kN/m
27 kN/m
12%
700%
22 kN/m
40 kN/m
12%
700%
29 kN/m
53 kN/m
12%
700%
Tear Resistance  (min. ave.)93N125 N187 N249 N
Puncture Resistance (min. ave.)240N320 N480 N640 N
Stress Crack Resistance (2)300 hr.300 hr.300 hr.300 hr.
Carbon Black Content - %2.0-3.0%2.0-3.0%2.0-3.0%2.0-3.0%
Carbon Black Dispersionnote (4)note (4)note (4)note (4)
Oxidative Induction Time (OIT) 
(min. ave.) (5)
(a) Standard OIT- or -
(b) High Pressure OIT
100 min.
400 min.
100 min.
400 min.
100 min.
400 min.
100 min.
400 min.
Oven Aging at 85°C (5), (6)
(a) Standard OIT (min. ave.) - % 
retained after 90 days- or -
(b) High Pressure OIT (min. ave.) - % retained after 90 days
55%
80%
55%
80%
55%
80%
55%
80%
UV Resistance (7)
(a) Standard OIT (min. ave.)- or -
(b) High Pressure OIT (min. ave.) - % retained after 1600 hrs
N.R. (8)
50%
N.R. (8)
50%
N.R. (8)
50%
N. R. (8)
50%v
Waterproofing HDPE Geo Membrane Pit Liner for Pond
Waterproofing HDPE Geo Membrane Pit Liner for Pond
Waterproofing HDPE Geo Membrane Pit Liner for Pond

Contact  us:Nanchang  Jubo  Engineering  Material Co., Ltd 
Nanchang Jubo Engineering Material Co., Ltd is one of the most experienced vendors for building materials.
Our company has established unique factories resources and sufficient inventory.
 We have received clients' favourable comments for the good quality and low price.
Waterproofing HDPE Geo Membrane Pit Liner for Pond

FAQ:

Q: Can I have a sample?

A: Yes, it is our pleasure to send free samples for checking quality and ?just undertake the?freight?charge by yourself.

Q:What is the lead time for samples?

A: Current sample need 1 day, customized samples need 5-7 days,

Q:What express do you use to send the samples?

A: We usually ship samples by DHL, TNT, FEDEX and UPS. It usually takes 3-5 days to arrive.

Q:What is the payment terms?

A: Our usual payment term is T/T and L/C . Others could be negotiated.

Q:Can you produce as my drawing?

A:Yes, we can customized for you?based on your drawing or sizes.

Q:How about the delivery time?

A:Usually production time is 10-15 days. It will be decided by the order quantity.

Contact us

Please feel free to give your inquiry in the form below We will reply you in 24 hours